SUBSTANCE, g/m2 |
CALIPER, μm |
BULK, cm3 /g |
BENDING STIFFNESS, mN (TAPP1 T 556) |
||
MD |
CD | GM | |||
TOL : ± 3% | TOL : ± 5% | TOL : ± 5% | TOL : ± 15% | ||
160 | 216 | 1.35 | 65 | 27 | 40 |
165 | 223 | 1.35 | 66 | 33 | 45 |
170 | 230 | 1.35 | 70 | 35 | 50 |
180 | 243 | 1.35 | 75 | 38 | 55 |
190 | 257 | 1.35 | 88 | 40 | 60 |
200 | 270 | 1.35 | 100 | 44 | 65 |
210 | 284 | 1.35 | 110 | 50 | 75 |
220 | 297 | 1.35 | 132 | 55 | 85 |
230 | 311 | 1.35 | 143 | 60 | 95 |
240 | 324 | 1.35 | 160 | 75 | 110 |
250 | 338 | 1.35 | 176 | 77 | 115 |
260 | 351 | 1.35 | 220 | 100 | 150 |
270 | 365 | 1.35 | 230 | 105 | 155 |
280 | 378 | 1.35 | 247 | 110 | 165 |
290 | 392 | 1.35 | 270 | 120 | 180 |
300 | 405 | 1.35 | 308 | 130 | 200 |
310 | 419 | 1.35 | 320 | 135 | 210 |
320 | 432 | 1.35 | 374 | 160 | 245 |
PROPERTY | TOLERANCE | VALUE | |||
MOISTURE, % |
(TAPPI T 412)
|
Up to 300 GSM
|
-
|
6.0 to 7.0 | |
Above 300 GSM
|
-
|
7.0 to 8.0 | |||
SMOOTHNESS, ml/min | (TAPPI T 555) |
Up to 300 GSM
|
Top / Bottom | Max | 250/600 |
Above 300 GSM | Max | 350/1000 | |||
PLYBOND, J/m2 | (TAPPI T 569) | - | Min | 200 | |
COBB60, g/m2 | (TAPPI T 441) | Top / Bottom | Max | 30/30 | |
BRIGHTNESS, % | (ISO 2469) | Top | Min | 83 | |
EDGE Wick, kg/m2 /hr | (IMS/U2/QC/SOP(13)) | - | Max | 1.50 |
Note: The results of the properties are as per TNPL lab test measurements according to International standard test methods - TAPPI/ISO. Conforming to BFR XXXVI, IS6615, US FDA 21.CFR.176.170 standards.